When you use CA it's a bit like mustard, you waste more than you actually use. You try to squeeze gently but it still comes out like the Amazon river, well it does for me anyway.
The tyres were CA's to the rims as they would not hold with the clamping system of the rims.
We came a across some PTFE tubing, CA does not stick to PTFE, the company is link
PTFE Tubing | Fluoroplastic Tubing & Rod | Adtech
They start at 0.01mm tubing. I used it today to put the glue inside an acrylic blank right where i wanted it with no waste and CA everywhere. I bought a 1m length, you only use 1cm at a time and you can clean it out and use it again.
Anyway just though i would share this, it may be helpful
The tyres were CA's to the rims as they would not hold with the clamping system of the rims.
We came a across some PTFE tubing, CA does not stick to PTFE, the company is link
PTFE Tubing | Fluoroplastic Tubing & Rod | Adtech
They start at 0.01mm tubing. I used it today to put the glue inside an acrylic blank right where i wanted it with no waste and CA everywhere. I bought a 1m length, you only use 1cm at a time and you can clean it out and use it again.
Anyway just though i would share this, it may be helpful